A423 GR.3 seamless tube is successfully delivered

Delivery for wear -resistant, acid -resistant dew point corrosion GR.3 The air heater is delivered in batches with seamless tubes
 
In mid -July, our company received the source of the source of a air -heater manufacturer. The other party urgently needed a batch of US standard A423 GR.3 air heater with seamless tubes. The product specifications were 40*1.5 and 50*2;
 
The manufacturer used to use welding steel pipes as tube. The equipment usage cycle was shorter than expected. This decision was decided to use seamless steel pipes to replace the original welding steel pipe, and to seamless steel pipes with high corrosion resistance and abrasion resistance.If a steel pipe is used in the process of using the air premier, the phenomenon of damage, cracking, leakage, and blocking during use will affect the overall operating efficiency of the equipment; the reason for the above phenomenon is that the fly ash in the flue gas is flushed and worn out the dew point after the temperature reaches the dew point. After the acid corrosion, SCR and SNCR are combined with the combination of departure, ammonia escapes and forms a pipeline of ammonium sulfate scale.
 
In response to the above situations and the standard requirements, our company decided to reasonably adjust the content of Ni, CU, MO and other elements in the pipeline, and adopt an oxidized light heat treatment process to seek products to obtain a comprehensive comprehensive in terms of wear -resistant and acid -resistant corrosion performance of acid dew point corrosion. promote. After more than two months of repeated research and trial production, in late September, our laboratory simulated related application environment, using a 50%H2SO4 test medium, the test temperature is set to 70 ℃ ± 2 ℃, the sample is soaked for 24 hours, and the sample is measured. See Table 1 at the corrosion rate; at the same time, other performance indicators of the sample tube have been recognized by equipment manufacturers. At present, this batch of GR.3 heater is delivered in batches with seamless steel pipes. Our company will continue to follow up the effect of the equipment to provide basic data support for the performance of steel pipes.

Table 1 Corrosion resistance
Test frequency 1 2 3 4 5 Average value
Corrosion rate G/㎡*H 34.81 37.22 35.67 34.21 36.02 35.59
 



Products categories

  • field:title/]

    Leaders' condolences - Special

  • field:title/]

    Den 30:e ryska internationella

  • field:title/]

    Our strong cooperation

  • field:title/]

    Strengthen the safety awareness

  • field:title/]

    Beite Steel Pipe New Apprentice

  • field:title/]

    Excellent Partner - Recognition

  • field:title/]

    New Product R & D--X20CRMov

  • field:title/]

    The standard approval meeting w